Biz yetkazib beramizko'priklar uchun-issiq prokatlangan ob-havoga chidamli po'latdir(masalan, Q355NH), turli uzunlikdagi ko'priklar va qattiq tashqi muhit uchun mo'ljallangan. Qalinligi 16 mm dan kam yoki unga teng bo'lsa, u 355 MPa dan katta yoki unga teng bo'lgan minimal oqish quvvatini va 490–630 MPa valentlikni ta'minlaydi, cho'zilish 22% dan katta yoki unga teng va 180 graduslik yaxshi egilish ko'rsatkichi.
Oddiy ko'prikli po'lat bilan solishtirganda, u o'xshash yoki yaxshiroq yuk ko'tarish qobiliyatini-ta'minlaydi, shu bilan birga korroziya bilan bog'liq bo'lim yo'qotilishini kamaytiradi-. Atmosfera, sanoat va qirg'oq muhitida u zich himoya zang qatlami hosil qiladi, korroziyaga chidamliligini uglerod po'latiga nisbatan taxminan 45% ga oshiradi.
Bu birinchi parvarishlash qoplamasini 15-20 yil yoki undan ko'proq vaqtga kechiktirishga imkon beradi, bu esa hayot aylanishiga texnik xizmat ko'rsatish xarajatlarini sezilarli darajada kamaytiradi. U ko'prik trusslarida, ark ko'prigi elementlarida, baland tuzilmalarda va og'ir-tashqi po'lat konstruktsiyalarda keng qo'llaniladi.


Biz GB/T 4171-2008 standartiga muvofiq, Q235NH, Q355NH va Q310GNH kabi navlarni oʻz ichiga olgan, turli uzunlikdagi koʻpriklar uchun turli yuk koʻtaruvchi talablarga javob beradigan-issiq prokatlangan yuqori nurashga chidamli koʻprik konstruktiv poʻlatini yetkazib beramiz.
An'anaviy ko'prik po'latlari (karbonli po'lat yoki havoga chidamli bo'lmagan past-po'lat) bilan solishtirganda, ular nam, korroziyali va tsiklik yuklanish muhitida zanglash, parchalanish va bo'laklarni yo'qotishga moyil bo'lgan GB/T 4171-2008 ob-havoga chidamli po'lat uzoq muddatli barqaror mexanik ish faoliyatini saqlaydi.
Qalinligi 16 mm dan kam yoki unga teng bo'lsa, Q355NH kabi asosiy navlar 355 MPa dan katta yoki unga teng bo'lgan minimal oquvchanlikni ta'minlaydi, Q310GNH esa 310 MPa dan katta yoki teng bo'lishini ta'minlaydi, charchoqqa mukammal qarshilik va sovuq shakllanish ko'rsatkichlari bilan. Oddiy xizmat ko'rsatish sharoitida uning strukturaviy xizmat muddati 30-50 yil yoki undan ko'proqqa uzaytirilishi mumkin, bu oddiy karbonli po'latdan yasalgan ko'prik konstruktsiyalaridan sezilarli darajada ustundir.
Magistral, temir yo'l va shahar ko'tarilgan ko'prik ilovalarida birinchi parvarishlash qoplamasi 15-20 yil yoki undan ko'proq vaqtga kechiktirilishi mumkin, umumiy xizmat muddati odatda an'anaviy karbonli po'lat konstruktsiyalarga nisbatan 2-3 baravar ko'p. Bu uzoq muddatli texnik xizmat ko'rsatish chastotasini, traffikni to'xtatish xavfini va bilvosita operatsion yo'qotishlarni sezilarli darajada kamaytiradi.
Ko'priklar uchun ob-havoga chidamli konstruktiv po'latning spetsifikatsiyasi
|
Element |
Spetsifikatsiya |
|
Mahsulot nomi |
GB/T 4171 Atmosfera korroziyasiga chidamli strukturaviy po'lat plitalar |
| Material darajasi | Q235NH, Q295NH, Q295GNH, Q355NH, Q355GNH, Q415NH, Q460NH, Q500NH, Q550NH, Q265GNH, Q310GNH) |
| Qalinligi diapazoni | 1,5 mm - 40,0 mm |
| Kenglik diapazoni | 1000 mm, 1250 mm, 1500 mm, 1800 mm, 2000 mm yoki moslashtirilgan |
| Uzunlik diapazoni | 2000 mm, 3000 mm, 6000 mm, 12000 mm yoki moslashtirilgan |
| Yuzaki holati | -Qaytirilgan, tuzlangan yoki oldindan-zanglangan (tezlashtirilgan havo bilan ishlov berish) |
| Ishlab chiqarish jarayoni | Issiq haddelenmiş, termo{0}}mexanik boshqaruv jarayoni (TMCP), normallashtirilgan |
| Qayta ishlash xizmatlari | Lazerli kesish, CNC zımbalama, bükme, payvandlash, tekislash |
| Chet holati | Tegirmon qirrasi (ME), Yoriq qirrasi (SE) |
| Yetkazib berish sharti | Issiq haddelenmiş / boshqariladigan haddelenmiş / normalizatsiya qilingan haddelenmiş |
| Sertifikat | UZ 10204 3.1 MTC, Tegirmon sinovi sertifikati |
| Tekshirish mavjud | PMI (Kimyoviy tahlil), Mexanik sinov, Ta'sir sinovi, SGS, BV, TUV |
| Yetkazib berish vaqti | 7-15 kun |
Ko'prik uchun GB / T 4171 ob-havoga chidamli strukturaviy po'latning kimyoviy tarkibi
| Baho | C (%) | Si (%) | Mn (%) | P (%) | S (%) | Cu (%) | Cr (%) | Ni (%) |
|---|---|---|---|---|---|---|---|---|
| Q235NH | 0,14 dan kam yoki teng | 0.20–0.50 | 0.30–0.65 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q265GNH | 0,14 dan kam yoki teng | 0.20–0.50 | 0.40–0.80 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q295NH | 0,13 dan kam yoki unga teng | 0.20–0.50 | 0.50–1.00 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q295GNH | 0,13 dan kam yoki unga teng | 0.20–0.50 | 0.50–1.00 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q310GNH | 0,13 dan kam yoki unga teng | 0.20–0.50 | 0.60–1.20 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q355NH | 0,12 dan kam yoki teng | 0.20–0.50 | 0.80–1.50 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q355GNH | 0,12 dan kam yoki teng | 0.20–0.50 | 0.80–1.50 | 0.060–0.120 | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.30–1.25 | 0,65 dan kam yoki unga teng |
| Q415NH | 0,12 dan kam yoki teng | 0.20–0.50 | 0.90–1.60 | 0,060 dan kam yoki unga teng | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.40–1.25 | 0,65 dan kam yoki unga teng |
| Q460NH | 0,12 dan kam yoki teng | 0.20–0.50 | 1.00–1.70 | 0,060 dan kam yoki unga teng | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.40–1.25 | 0,65 dan kam yoki unga teng |
| Q500NH | 0,12 dan kam yoki teng | 0.20–0.50 | 1.20–1.80 | 0,060 dan kam yoki unga teng | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.40–1.25 | 0,65 dan kam yoki unga teng |
| Q550NH | 0,12 dan kam yoki teng | 0.20–0.50 | 1.20–1.80 | 0,060 dan kam yoki unga teng | 0,030 dan kam yoki unga teng | 0.25–0.55 | 0.40–1.25 | 0,65 dan kam yoki unga teng |
Ko'prik uchun GB / T 4171 ob-havoga chidamli strukturaviy po'latning mexanik xususiyatlari
| Baho | Hosildorlik kuchi ReH (MPa) | Kuchlanish kuchi Rm (MPa) | Cho'zilish A (%) | Ta'sirga chidamliligi |
|---|---|---|---|---|
| Q235NH | 235 dan katta yoki teng | 360–500 | 26 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q265GNH | 265 dan katta yoki teng | 400–520 | 25 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q295NH | 295 dan katta yoki teng | 420–540 | 24 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q295GNH | 295 dan katta yoki teng | 420–540 | 24 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q310GNH | 310 dan katta yoki teng | 440–570 | 23 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q355NH | 355 dan katta yoki teng | 490–630 | 22 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q355GNH | 355 dan katta yoki teng | 490–630 | 22 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q415NH | 415 dan katta yoki unga teng | 520–680 | 20 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q460NH | 460 dan katta yoki unga teng | 550–720 | 19 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q500NH | 500 dan katta yoki unga teng | 610–760 | 17 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |
| Q550NH | 550 dan katta yoki unga teng | 620–780 | 16 dan katta yoki teng | 20 daraja 27J dan katta yoki teng |




GB/T 4171 Weathering Steelning ekvivalent navlari
| GB/T 4171 darajasi | EN standarti (Evropa) | ASTM (AQSh) | JIS (Yaponiya) |
|---|---|---|---|
| Q235NH | S235J0W / S235J2W | ASTM A242 | SPA-H (pastki diapazon) |
| Q265GNH | S275J0W | ASTM A242 / A588 (past) | SPA-H |
| Q295NH | S355J0WP (taxminan past) | ASTM A242 | SPA-H |
| Q295GNH | S355J0WP | ASTM A588 A darajasi | SPA-H |
| Q310GNH | S355J2W (yaqin o'yin) | ASTM A588 A darajasi | SPA-H |
| Q355NH | S355J0WP / S355J2W | ASTM A588 B darajasi | SPA-H |
| Q355GNH | S355J2W | ASTM A588 B darajasi | SPA-H |
| Q415NH | S420W (taxminan) | ASTM A588 B/C darajasi | SPA-H (yuqori quvvat) |
| Q460NH | S460W (taxminan) | ASTM A588 C darajasi | SPA-H (yuqori quvvat) |
| Q500NH | S500W (taxminan) | ASTM A588 K darajasi (yaqin) | SPA-H tahrirlangan |
| Q550NH | S550W (taxminan) | ASTM A588 K / A709 darajasi | SPA-H tahrirlangan |
Qo'llash ishi: Ob-havoga chidamli po'lat ko'priklar

Thames Valley Parkway – Shimoliy filiali - London, ON
Egasi: London shahri
Qo'llash sohasi: dizayn, ishlab chiqarish, yetkazib berish va o'rnatish

Whirlpool Road Multi-Use Pathway Piyodalar ko'prigi - Niagara, ON
Egasi: Niagara sharsharasi shahri
Qo'llash sohasi: dizayn, ishlab chiqarish, yetkazib berish va o'rnatish

Rowntree Mills Park Shimoliy ko'prigi va yo'lini reabilitatsiya qilish - Shimoliy York, ON
Egasi: Toronto shahri
Qo'llash sohasi: dizayn, ishlab chiqarish, yetkazib berish va o'rnatish
Ob-havoga chidamli po‘lat ko‘priklar qoplamaning nol-vaqt aylanishiga ega bo‘lib, bu nafaqat maydonda püskürtme{1}}bo‘lgan VOC emissiyasini yo‘qotibgina qolmay, balki qoplama jarayonini butunlay o‘tkazib yuborib,-ko‘prik ustki tuzilmasini qurish vaqtini 20% dan ortiq qisqartiradi.
Bepul poʻlat koʻpriklarni qoplash-uchun toʻliq dizayn va tezkor qurilish rejasini olish uchun bugun biz bilan bogʻlaning!
Corten Steel Bridge taklifini olish uchun hozir bog'laning
GNEE Steel po'latdan yasalgan ko'prik muhandisligi bo'yicha keng qamrovli xizmatlarni taklif qilish uchun to'liq jihozlangan og'ir yuklarni qayta ishlash markazlarini boshqaradi:
Nozik kesish va kesish:
Yuqori{0}}kuchli lazerli kesish, CNC plazma bilan kesish va olovda kesish (maxsus-50 mm+ gacha bo'lgan yuqori quvvatli og'ir plitalar uchun optimallashtirilgan). Biz keyingi ko'prik yig'ish uchun mukammal mosligini ta'minlash uchun yuqori aniqlikdagi trubalarni qayta ishlashni (V, X, Y turlari) ta'minlaymiz.




Yuzaki ishlov berish-:
Tegirmon shkalasini butunlay olib tashlash uchun ilg'or avtomatik portlatish (Sa2.5/Sa3.0 tozalik standartiga erishish). Biz, shuningdek, bir necha kun ichida bir xil, zich himoyalovchi zang qatlamini (Fe3O4) hosil qilish uchun-ekologik toza kimyoviy tezlashtirilgan ob-havo bilan ishlov beramiz, bu esa tirgaklarda zangning erta bo'yalishini oldini oladi.

Og'ir shakllantirish va tekislash:
Katta{0}}tonajli CNC egilish, plastinka tekislash (ichki burilish kuchlanishini bartaraf etish) va nozik prokat, U-qovurg‘alar, quti to‘sinlar va kavisli ko‘prik konstruktiv komponentlari uchun juda mos keladi.


Mos keladigan payvandlash va quyi{0}}montaj:
Zavodda boshqariladigan-avtomatlashtirilgan qoʻshimcha yigʻish va payvandlash boʻyicha maxsus ob-havoga chidamli payvandlash materiallaridan foydalanish xizmatlari. Bizning jarayonlarimiz AWS, EN va uchinchi tomon tekshiruvi (SGS/BV)-standartlariga mos keladigan, atmosfera korroziyaga chidamliligi va asosiy metallning past haroratga{3}}tasirchanligiga qat'iy mos keladi.
Corten Steel Bridge-ning yetkazib berish vaqti
Standart zaxira:
Ko'prikning ob-havoga chidamli po'latning umumiy texnik xususiyatlari (masalan, A588/SPA-H/Q355NH, qalinligi 6 mm–40 mm, kengligi 1500 mm/2000 mm/2500 mm) uchun doimiy inventarizatsiya saqlanadi.
Yetkazib berish:Mahsulotlar oldindan to'lov yoki akkreditiv (L/C) olingandan keyin 3 dan 7 ish kunigacha qayta ishlanishi, ombordan jo'natilishi va jo'natishga tayyor bo'lishi mumkin.
Moslashtirilgan / Maxsus spetsifikatsiyalar:
Qo'shimcha kenglik (3500 mm+ gacha), qo'shimcha qalinlik (50 mm–100 mm+), qattiq Z-yo'nalishi bo'yicha ishlash (Z15/Z25/Z35) yoki maxsus ishlov berish (masalan, payvandlashdan oldingi portlatish/) talab qilinadigan og'ir plitalar uchun ishlab chiqarishni rejalashtirish buyurtmalari to'g'ridan-to'g'ri po'lat tegirmonlarga berilishi kerak.
Yetkazib berish:Yetkazib berish muddati odatda tegirmonning ishlab chiqarish jadvali va loyiha hajmiga qarab 20 dan 35 ish kunigacha.
Sinov va tekshirishko'priklar uchun konstruktiv po'latni nurash
MTC (material sinovi sertifikati):
EN 10204 3.1 yoki 3.2 standartlariga mos keladigan materiallarning toʻliq sinov sertifikatlarini taqdim etadi. MTC batafsil kimyoviy tarkibni (shu jumladan Cu, Cr, Ni, P kabi asosiy ob-havo elementlarini) va aniq mexanik xususiyatlarni (oqim kuchi, valentlik kuchi, cho'zilish) qamrab oladi.
Past-harorat ta'siriga chidamlilik sinovi:
Sovuq iqlim sharoitida mo'rt sinishning oldini olish uchun Charpy V{0}}cho'qqisining zarba energiyasini belgilangan haroratlarda (masalan, 0 daraja , -20 daraja yoki -40 daraja ) sinovdan o'tkazish ko'prik xavfsizligi uchun juda muhimdir.
Ultratovush tekshiruvi (UT):
ASTM A435/A578 yoki EN 10160 standartlariga muvofiq, ichki nuqsonlarni, laminatsiyalarni yoki bo'shliqlarni aniqlash uchun og'ir ko'prik plitalari uchun bajariladi, bu strukturaning yaxlitligini ta'minlaydi.
Z-Yoʻnalish (qalinligi-boʻylab) kuchlanish sinovi:
Og'ir ko'prik ishlab chiqarish va payvandlashda lamellar yorilishining oldini olish uchun qalin payvandlangan qismlar uchun so'rov bo'yicha (Z15/Z25/Z35) mavjud.
Atmosfera korroziyasi indeksi (I-qiymat) tekshirish:
Uzoq muddatli ob-havo va korroziyaga qarshi-yuqori ko‘rsatkichlarni kafolatlash uchun issiqlik tahlili asosida ob-havoga chidamli po‘lat korroziya indeksini hisoblab chiqadi.
Uchinchi{0}tomon tekshiruvi:
Uchinchi tomon tekshiruvlari-(masalan, SGS yoki Bureau Veritas) toʻliq qoʻllab-quvvatlanadi.