Corten Steel Dging haqida tez-tez so'raladigan savollar

Dec 02, 2025 Xabar QOLDIRISH

Corten Steel Edge nima? Nima uchun foydalaniladi?

 

Korten po'latdan yasalgan chekka, shuningdek, metall landshaft chekkasi sifatida ham tanilgan, gulzorlar, maysazorlar, yo'llar yoki boshqa landshaft dizayni xususiyatlari kabi bog'ning turli joylari o'rtasida aniq ajratishni yaratish uchun ishlatiladi. U ixcham joyga o'rnatiladi va bog'ning toza, tartibli tartibini saqlashga yordam beradi.

Corten steel edging

Corten po'latdan yasalgan chetidan foydalanish funktsional va estetik jihatdan bir nechta afzalliklarni beradi. Vaqt o'tishi bilan po'latdan issiq apelsin{1}}qo'ng'ir rangli patina paydo bo'lib, u tabiiy ravishda tashqi muhit bilan uyg'unlashadi. Uning rustik va ob-havoga chidamli ko'rinishi bog 'dizaynlarining umumiy vizual jozibasini oshiradi va turli xil peyzaj xususiyatlarini to'ldiradi.

 

Corten Edgingning ishlash muddati qancha?

 

Corten po'latdan yasalgan qirralarning ishlash muddati atrof-muhit sharoitlariga, po'latning qalinligiga va texnik xizmat ko'rsatish amaliyotiga bog'liq. Ajoyib chidamliligi va korroziyaga chidamliligi tufayli, to'g'ri o'rnatilgan va parvarish qilingan{1}}Corten po'lat qirralari 20 yildan 50 yilgacha-ba'zi hollarda undan ham uzoqroq xizmat qilishi mumkin. Uning tabiiy ravishda hosil bo'lgan himoya patinasi po'latni keyingi korroziyadan himoya qilishga yordam beradi va uning uzoq-foydalanishiga hissa qo'shadi.

 

Korten po'latdan yasalgan bog 'chekkasini egishingiz mumkinmi?

 

Ha, Corten po'latdan yasalgan bog 'qirrasi egri chiziqlar va maxsus dizaynlarni yaratish uchun shakllantirilishi va egilishi mumkin. Po'lat egiluvchan bo'lib, yorilish yoki sindirmasdan egilishi mumkin, bu uni obodonlashtirish uchun juda ko'p qirrali qiladi.

 

Zanglagan po'latni ma'lum bir haroratga qizdirish orqali bog 'yotoqlari, yo'llar va boshqa tashqi xususiyatlar uchun silliq, oqadigan qirralarning hosil bo'lishi osonroq bo'ladi. Ushbu moslashuvchanlik landshaftchilar va bog'bonlarga ham funktsional, ham estetik jihatdan yoqimli tartiblarga erishishga imkon beradi.

 

Corten po'lat qirralarning spetsifikatsiyasi

 

Ko'rsatkichlar Qalinligi Uzunlik
Ko'rsatkich 14, 11 1,5 dan 3 mm gacha 2400 mm gacha
Standart Foydalanadi Balandligi
a606-4 chegaralar va to'shaklar
maysazor chekkasi
100 dan 300 mm gacha

 

Corten po'latdan obodonlashtirish o'lchov diapazoni

 

Yuqori chekka turi Yuqori katlama yo'q, 50 mm - 90 daraja, 25 mm - 90 daraja, xavfsizlik chekkasi - 180 daraja
Balandligi 300mm, 150mm, 100mm, 200mm, 400mm
Materialning qalinligi 3 mm, 2 mm
Tab konnektori Yo'q, Ha

 

Korten metall qirralarning o'lchovi va o'lchamlari

 

Peyzaj qirralari Peyzaj qoziqlari (11 kalibr) Landshaft qoziqlari (14 kalibr) Peyzaj burchaklari
14 gauge, 6 dyuym x 120 dyuym 11 gauge, 10 ″ umumiy (6″ yuzni qoplash) 14 gauge, 10 ″ umumiy (6″ yuzni qoplash) 11 kalibr, 12 dyuym
14 gauge, 4" x 120" 11 kalibr, 8 ″ umumiy (4″ yuzni qoplash) 14 gauge, 8 ″ umumiy (4″ yuzni qoplash) 11 kalibr, 6 dyuym
14 gauge, 12" x 120" 11 kalibr, 16 ″ umumiy (12 ″ yuzni qoplash) 14 gauge, 16 ″ umumiy (12 ″ yuzni qoplash)  
14 gauge, 8 dyuym x 120 dyuym 11 kalibr, 12 ″ umumiy (8″ yuzni qoplash) 14 gauge, 12 ″ umumiy (8″ yuzni qoplash)  
11 gauge, 6 dyuym x 120 dyuym      
11 gauge, 12" x 120"      
11 gauge, 4" x 120"      
11 gauge, 8 dyuym x 120 dyuym      

 

Corten po'lat landshaft chekka mexanik xususiyatlari

 

  Metrik Imperator
Eng yuqori kuchlanish kuchi 483 MPa 70,000psi
Zichlik 7,75 g/cc 0,28 funt/in3
Chiqish quvvati 345 MPa 50,000psi

 

Corten qirrasi ekvivalenti

 

Material # ASTM SEW 087 EN 10155 UNI NFA 35-502 BS 4360 JIS G3114
1.8967 S355K2G2W
1.8945 E 36 WA 3 S355J0WP WR 50 A Fe 510 C1K1
1.8961 WTSt 37-3 S235J2W Fe 360 ​​DK 1 E 24 W 4
1.8959 A 588 – A 242 Gr. 1 S355J0W Fe 510 C2K1 E 36 WB 3 WR 50 B SMA 50 AW
1.8946 A 242 1-turi S355J2WP Fe 510 D1K1 E 36 WA 4
1.8965 S355J2G2W SMA 50 CP
1.8963 588 gr. A WTSt 52-3 S355J2G1W Fe 510 D2K1 WR 50 C uchun
1.8966 709 Gr. 50 Vt S355K2G1W E 36 WB 4

 

Korten po'latdan yasalgan bog 'chekka kimyoviy xossalari

 

  Si %
maks.
C %
maks.
Mn % Z% S %
maks.
P % N %
maks.
Cr % V% Cu % Ni% Mo%
EN 10027-1 va CR 10260 ga muvofiq
S235J2W 0.40 0.13 0.20-0.60 0.03 0.04 0.40-0.80 0.25-0.55 0.65
S235J0W 0.40 0.13 0.20-0.60 0.04 0.04 0.01 0.40-0.80 0.25-0.55 0.65
S355J2WP 0.75 0.12 1.00 0.03 0.06-0.15 0.30-1.25 0.25-0.55 0.65
S355J0W 0.75 0.12 1.00 0.04 0.06-0.15 0.01 0.30-1.25 0.25-0.55 0.65
S355J2W 0.50 0.16 0.50-1.50 0.15 0.03 0.03 0.40-0.80 0.25-0.55 0.65 0.30
S355J0W 0.50 0.16 0.50-1.50 0.15 0.04 0.04 0.01 0.40-0.80 0.25-0.55 0.65 0.30
S355K2W 0.50 0.16 0.50-1.50 0.15 0.03 0.03 0.40-0.80 0.25-0.55 0.65 0.30
ASTM & ASME Specn ma'lumotlariga ko'ra.
588 gr. B 0.15-
0.50
0.20 0.75-1.35   0.05 0.04 0.40-0.70 0.01-
0.10
0.20-0.40    
588 gr. A 0.3-
0.65
0.19 0.80-1.25   0.05 0.04 0.40-0.65 0.02-
0.10
0.25-0.40    
588 gr. C 0.15-
0.40
0.15 0.80-1.35   0.05 0.04 0.30-0.50 0.01-
0.10
0.20-0.50    
A 242 turi-1 0.15 1.00   0.05 0.15       0,20 min.    
588 gr. K 0.25-
0.50
0.17 0.50-1.20 Cb-0,005
-0.05
0.05 0.04 0.40-0.70 0.30-0.50    
A 242 turi-2 0.20 1.50   0.05 0.04       0,20 min.    
IS STD ma'lumotlariga ko'ra.
IRSM-41 0.30-
0.50
0.10 0.25-0.45 0.03 0.075-0.14 0.35-0.49 0.05 0.30-0.60 0.28-
0.49
0.05

 

Corten Landscape Edge-ning afzalliklari qanday? U texnik xizmat ko'rsatishni talab qiladimi?

 

Corten po'lati tabiiy ob-havoga ega bo'lib, bog 'chegaralariga rustik va organik estetika qo'shadi.

Material juda bardoshli va korroziyaga chidamli bo'lib, uni tashqi makon uchun ideal qiladi.

Korten po'latdan yasalgan landshaft chekkalaridagi tabiiy shakldagi patina ham ko'rinishda jozibali, ham -parcha parvarish talab etilmaydi.

U osongina egilib yoki shakllantirilishi mumkin, bu ijodiy va moslashuvchan qirralarning dizaynlarini yaratishga imkon beradi.

Korten ekologik toza material bo'lib, u qayta ishlanishi va qayta ishlatilishi mumkin.

 

Corten landshaft chekkasi minimal parvarishlashni talab qiladi. Muntazam tekshiruvlar va engil tozalash chiqindilarni olib tashlashga va yuzaga kelishi mumkin bo'lgan muammolarni oldini olishga yordam beradi, chekka eng yaxshi ko'rinishini saqlaydi.

 

Ob-havoga chidamli po'latdan qirrani qanday o'rnatish kerak

 

Zaminni tekislash va uni qoldiqlardan tozalashdan keyin chekka uchun joyni o'lchab, belgilang.

Belgilangan chiziq bo'ylab sayoz xandaq qazing.

Kenar uchun mustahkam asos yaratish uchun xandaqqa siqilgan shag'al yoki qum qatlamini qo'ying.

Zanglagan metall bog 'chekkasini (Corten po'lati) xandaqqa joylashtiring. Uning tekisligiga va mo'ljallangan chegaraga mos kelishiga ishonch hosil qiling.

Doimiy vaqt oralig'ida qoziqlar yoki langarlar yordamida chekkalarni mahkamlang.

Xandaqni tuproq bilan to'ldiring, uni mahkam ushlab turish uchun chekka atrofida siqib qo'ying.

Ortiqcha tuproqni olib tashlang va Gnee Corten po'lat qirrasi vizual ravishda tekis va tekis ekanligini tekshiring.

 

Zanglangan po'latdan yasalgan bog 'qirrasi qancha turadi?

 

Zanglagan po'latdan yasalgan bog 'chekkasining narxi etkazib beruvchiga qarab farq qiladi va Corten po'latining narxiga va bozor sharoitlariga bog'liq. Raqobatbardosh narxda eng yaxshi sifatli chekka uchun, moslashtirilgan narx uchun Gnee Steel korporatsiyasi bilan bog'laning.

 

Hozir bog'laning

 

info-574-733